search  current discussion  categories  kilns & firing - misc 

fb firing schedule

updated fri 1 apr 05

 

Dinah Collopy on thu 31 mar 05


I just finished doing six test pieces (all textured) with Floating Blue.
I made up three different glazes, the original from Chappell , Ron's =
first reformulation with some GB and some Frit 3134 and his latest with =
no GB, just 3134.
I fired the first batch using the ramp and hold on the computer and =
followed the newest schedule recommend by John for the glazes in =
"Mastering Cone 6 Glazes".
The second batch I fired just using the cone firing setting. I fired to =
cone 6 at medium speed and no hold.
The second batch was MUCH nicer.
Dinah
Mississippi Gulf Coast