What a great idea!! I mainly use Copper Sand, Copper Penny and White
Crackle.

Here is one I have used several times. I have used it on top of many
different glazes with nice results.





Gerstley Borate 500
Nepheline syenite 200
Barium Carbonate 200
Frit 3134 100
Cobalt Carb 10
Copper Carb 20

Deb