i put the wrong cones in the kiln - should i abort!!!

updated fri 6 may 05

 

Scott & Vanessa on wed 4 may 05


Hi all,

In a fog - I put 3 plaques of cone 05,04,03 into a kiln that is firing to
cone6. It's computer controlled so these are all just witness cones. But
I realized that I don't know what will happen to these cones, will they
turn into a liquid and drip off the shelves? I am totally clueless.
Please let me know soon so I can abort the firing before it's too late.

Thanks,

Scott and Vanessa

Snail Scott on thu 5 may 05


At 09:51 PM 5/4/2005 -0400, you wrote:
>Hi all,
>
>In a fog - I put 3 plaques of cone 05,04,03 into a kiln that is firing to
>cone6...will they
>turn into a liquid and drip off the shelves?


They will get drippy, yes, but won't flow like water.
If you have a good coating of kilnwash on the shelf
under them, they should come loose even after they melt.

-Snail

Gary Harvey on thu 5 may 05


I would you can always start it back.
----- Original Message -----
From: "Scott & Vanessa"
To:
Sent: Wednesday, May 04, 2005 8:51 PM
Subject: I put the wrong cones in the kiln - should I abort!!!


> Hi all,
>
> In a fog - I put 3 plaques of cone 05,04,03 into a kiln that is firing to
> cone6. It's computer controlled so these are all just witness cones. But
> I realized that I don't know what will happen to these cones, will they
> turn into a liquid and drip off the shelves? I am totally clueless.
> Please let me know soon so I can abort the firing before it's too late.
>
> Thanks,
>
> Scott and Vanessa
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>