Dan Saultman on mon 16 may 05


Hi guys,
I would like to invite you to visit my new updated web site page with
glazes developed using recipes and formulas from June Perry. Her
recipes are reliable and perform well. She is a regular contributor to
Clay Times.

My firing was flawed since I shut down a bit early ( 2243 cones 9 down
flat ) I got a toasty reduction/oxidation out of the firing but some of
the pieces were a bit under fired or immature. But it took me 16 hrs.
to get there.

Please visit my site (use this link below to click on) and view the
new mugs.
I'll be glad to share my glazes with anyone.

Best wishes to all in the group.

http://www.saultman.com/buy.html

Dan

Dan Saultman
Detroit
http://www.saultman.com