In a message dated 4/29/2005 7:35:47 PM Eastern Standard Time,
ronroy@CA.INTER.NET writes:
It adds up to to 107 - am i working with the right numbers?

RR


> I'm doing a study of Ferguson's Yellow, one of my favorite glazes. I
>have one recipie, and would like to know if anyone has a different one.
>Mine is
>
>custer 44
>kaolin 21
>dolomite 14
>whiting 9
>zircopax 9
>bone ash 7
>red iron ox 1
>bentonite 2
>
>I would greatly apprieciate any and all information on this glaze,
>formulas, historical info, whatever.
>
>thanks gregg

Ron Roy


Did anyone resolve this?
And is this Oxidation or reduction?
Thanks
Sincerely,
Susan