search  current discussion  categories  glazes - misc 

=?iso-8859-1?q?re:_=a0_=a0_=a0_nutmeg_glaze?=

updated mon 6 jun 05

 

Rose on sun 5 jun 05


At 08:08 AM 6/5/2005 , you wrote:

> -Richard Busch/Glenfiddich Farm Pottery, Leesburg, VA
> PS: In my original article, I noted that I used Std 112 because of the
>granular manganese that gives that nice speckly look. The editors cut that
>part, I assume so as not to offend other clay manuracturers by mentioning
>one (a
>wrongheaded policy, in my opinion).

My first test of this glaze I was using goldstone, a cone 6 clay from
Seattle Pottery. That clay has dark specks in it. I love this glaze. Thanks
for sharing it.

Rose from rainy Camano Island.