search  current discussion  categories  glazes - cone 4-7 

michael bailey c6 jb1 scaling,peeling off before firing

updated mon 6 jun 05

 

Cor Duijnker on sun 5 jun 05


My JB1 glaze is peeling off.
It peels off after it has dried on the pot, before firing.
I spray my glazes.
I also tried to spray my pots with water to wetten it a bit, but the =
problem isn't solved.

This is the recipe!

42.8 Soda Felspar
4.8 china cly
1.9 lithium carbonate
1.9 bentonite
16.2 whiting
4.8 zincoxide
22.8 quarts
4.8 titanium dioxide
1 cobaltcarbonate

I use a stoneware claybody bisque at 950 Celcius ( 1750F ) and I always =
use some wallpaper glue in the water, I use for my glaze.
It seems to be the glaze recipe,but can't find the problem.

Ron Roy on sun 5 jun 05


Hi Cor,

Let me know what kinds of ball clays you have or can get - if you are not
in North America - I will need the analysis as well.

RR

>My JB1 glaze is peeling off.
>It peels off after it has dried on the pot, before firing.
>I spray my glazes.
>I also tried to spray my pots with water to wetten it a bit, but the
>problem isn't solved.
>
>This is the recipe!
>
>42.8 Soda Felspar
>4.8 china cly
>1.9 lithium carbonate
>1.9 bentonite
>16.2 whiting
>4.8 zincoxide
>22.8 quarts
>4.8 titanium dioxide
>1 cobaltcarbonate
>
>I use a stoneware claybody bisque at 950 Celcius ( 1750F ) and I always
>use some wallpaper glue in the water, I use for my glaze.
>It seems to be the glaze recipe,but can't find the problem.


Ron Roy
RR#4
15084 Little Lake Road
Brighton, Ontario
Canada
K0K 1H0
Phone: 613-475-9544
Fax: 613-475-3513