Marta Matray Gloviczki on fri 3 jun 05
hi betty,
a year ago we on clayart lost a friend,
ababi sharon who lived in a kibbutz in israel.
he called himself a glaze addict, and
had an electric kiln. he made hundreds of
tests and found some electric fired glazes,
which looked similar to some shinos.
i think ababi's website is still on, if
someone can help... please.
ababi had pictures of many glaze tests,
and he had the recipes there too.
best,
marta
>A friend of mine loves the look of shino glazes but has an electric kiln.
>Does anyone have a recipe for a shino-like glaze at Cone 6 to 8 oxidation?
>She will be grateful for any suggestions.
=====
marta matray gloviczki
rochester,mn
http://www.angelfire.com/mn2/marta/
http://users.skynet.be/russel.fouts/Marta.htm
http://www.silverhawk.com/crafts/gloviczki/welcome.html
Israel Shmueli on sat 4 jun 05
Ababi's web site is still accessible.
http://members4.clubphoto.com/ababi306910/guest-1.phtml
Israel Shmueli
http://www.botzpottery.co.il
Lee Love on sat 4 jun 05
Marta Matray Gloviczki wrote:
>someone can help... please.
>ababi had pictures of many glaze tests,
>and he had the recipes there too.
>
ttp://members4.clubphoto.com/ababi306910
http://www.matrix2000.co.nz/Matrix%20Demo/Ababi.htm
His main web page doesn't work any longer, but I found it in the
internet archives:
http://tinyurl.com/18r
If you find any other non working links, go here and see if you can find
them in the archive:
http://www.archive.org/
--
李 Lee Love 大
愛 鱗
in Mashiko, Japan http://mashiko.org
http://hankos.blogspot.com/ Visual Bookmarks
http://ikiru.blogspot.com/ Zen and Craft
"With Humans it's what's here (he points to his heart) that makes the difference. If you don't have it in the heart, nothing you make will make a difference." ~~Bernard Leach~~ (As told to Dean Schwarz)
| |
|