turquoise crackle glaze cone 6

updated wed 6 jul 05

 

Andie Plamondon on sun 3 jul 05


Several years ago I mixed a batch of a cone 6/7 transparent turquoise
crackle glaze (electric fired).

Runs like mad, but gorgeous color. Just foot EVERY pot.

Well, I used the last of it & can't find the recipe - makes me wonder if I
was trying for something else, it may have been an accident.

I have some pictures of this glaze on my website, under the portfolio link -
www.handfulofearth.com

Anyone have a top-notch, dependable, truly turquoise crackle cone 6 glaze
like this to share?

I appreciate it -

:) Andie Plamondon
Handful of Earth Pottery
www.handfulofearth.com

Alisa Liskin Clausen on tue 5 jul 05


On Sun, 3 Jul 2005 15:36:32 -0400, Andie Plamondon wrote:

>Several years ago I mixed a batch of a cone 6/7 transparent turquoise
>crackle glaze (electric fired).
>
>Runs like mad, but gorgeous color. Just foot EVERY pot.
>
>


Top notch dependable, cannot say what would fit your parameters, however,
sounds like many a Alkaline Clears with 3% Cu added. They are often a
lovely celedon, turquoise and craze and run often. If you check the
archives, you will find glazes like this where I note that they crazed.

regards from Alisa in Denmark