Could anyone recommend methods of brick repair? Can I just glue cracked
bricks back together? What should I use?

I bought a soft brick kiln. I disassembled it and moved it to its new
location where it is to be reassembled. Half the bricks are cracked in
2 to 4 pieces, but I kept them in whole brick units and have them
stored indoors. The kiln is gas fired catenary arch type.