Sincultura 13 on sat 16 jul 05
Hi Everybody,
What precautions should I take when dipping greenware in slip/engobe so the pots don't crack?
Also is there any guidelines on how much flux can a slip/engobe take at cone 04-02 range before it starts sticking to the shelf?
Can I dip in glaze after dipping in slip/engobe wihtout firing the pots first?
I would prefer to dip the pots at bone dry stage...
Any tips, suggestions, links, etc... greatly appreciated.
Regards,
Sincultura
---------------------------------