C.C. Bookout on wed 20 jul 05


Does anyone know of a potter using this clay body? I am using it for
some hand coiled garden sculpture/vessels. The pieces are large and
have about 100 pounds of clay in them. I have a gas kiln and was
wondering about a firing and reduction scedule for firing these pieces.
Any feedback on this clay body would be a help. I loved working with it
and it seems so strong. I am just worried about the firing. Again the
clay body is standad 380 outdoor sculpture clay.