Is it possible to bonfire non bisqued papercrete (with grog) tiles.
Is it worth the effort?
Thanks,Sasha
William & Susan Schran User on sat 30 jul 05
On 7/30/05 6:39 AM, "Sasha" wrote:
> non bisqued papercrete (with grog) tiles.
What is papercrete? Do you mean paper clay?
Yes, you can put them in a bonfire.
Totally dry, at bottom of fire, covered with shards of fired clay or pieces
of metal.
--
William "Bill" Schran
Fredericksburg, Virginia
Sasha on mon 1 aug 05
> non bisqued papercrete (with grog) tiles.
What is papercrete? Do you mean paper clay?
Yes, you can put them in a bonfire. Totally dry, at bottom of fire, covered
with shards of fired clay or pieces of metal.
Sorry,mistake.Paperclay is what I wanted to say.Papercrete is a cement-paper
mix.
Can you explain it a little bit more?Have you try something like this?
Thanks ,Sasha
William & Susan Schran User on mon 1 aug 05
On 8/1/05 6:17 PM, "Sasha" wrote:
> Sorry,mistake.Paperclay is what I wanted to say.Papercrete is a cement-paper
> mix.
> Can you explain it a little bit more?Have you try something like this?
Yes, I've fired paperclay in pit firing, sawdust firing and in raku.
Rather than going into a lengthy explanation of each technique, I'd suggest
you do a web search for "pit firing" and you'll find many sites with
explanations and images.
--
William "Bill" Schran
Fredericksburg, Virginia
Sasha on tue 2 aug 05
Yes, I've fired paperclay in pit firing, sawdust firing and in raku.
Rather than going into a lengthy explanation of each technique, I'd suggest
you do a web search for "pit firing" and you'll find many sites with
explanations and images.
Yes, I have done the search many many times ,but havent seen anything about
pit firing of tiles.
Sasha
| |
|