Earl Brunner on wed 3 aug 05


Get one of Tom Coleman's glaze books, ALL of his glazes (just about) are for
white or off white clays.

Earl Brunner
Las Vegas, NV

-----Original Message-----
From: Clayart [mailto:CLAYART@LSV.CERAMICS.ORG] On Behalf Of Julie Moore
Sent: Wednesday, August 03, 2005 1:14 PM
To: CLAYART@LSV.CERAMICS.ORG
Subject: B-mix question

Hi,

I'm an old ClayArter returning after a long hiatus to ask a question. I've
fallen in love with the throwing qualities of B-mix (^10), but am not
thrilled with how boring my glazes look on it despite reduction firing.
Does anyone have glaze recipes they'd be willing to share that look good on
white clays, B-mix in particular?

Thanks,
Julie
Dirty Bird Pottery
www.dirtybirdpottery.com

Julie Moore on wed 3 aug 05


Hi,

I'm an old ClayArter returning after a long hiatus to ask a question. I've
fallen in love with the throwing qualities of B-mix (^10), but am not
thrilled with how boring my glazes look on it despite reduction firing.
Does anyone have glaze recipes they'd be willing to share that look good on
white clays, B-mix in particular?

Thanks,
Julie
Dirty Bird Pottery
www.dirtybirdpottery.com

Julie Moore on thu 4 aug 05


Thanks to Earl and Rosanne for the suggestion. I will definitely check out
the book.

Julie