search  current discussion  categories  books & magazines - books 

rhodes 32....a bit of a change for simplicity ended up being very

updated wed 10 aug 05

 

Bob Hanlin on mon 8 aug 05

good...

I changed the text book glaze to simplify the mixing and it turned out to be great for me.

Potash Feldspar..................45
Kaolin.................................25
Dolomite.............................25
Whiting.................................5

As I said in my last post, I used 1% iron and manganese.