pdp1@EARTHLINK.NET on mon 15 aug 05


Hi Ingeborg,


Likely, it is the moisture-cycle of the Wood - absorbing ambient humidity,
then drying when you fire, which is adversely effecting the quality of
adhesion of the Paint.


Phil
Las Vegas


----- Original Message -----
From: "Ingeborg Foco"

> Mel,
>
> My roof decking is ordinary rough sawn plywood and the support beams are
> some kind of engineered laminated beam. The paint failed first on the
beam
> and now all over the plywood as well. I do not have pressure treated
lumber
> up on the ceiling just the framework holding the bug screens is pressure
> treated.

<<<>>>

> Ingeborg