bonnie staffel on wed 17 aug 05
Dear Ama,
I add 1 to 1 mix of frit 3134 to Mason Stain as well as some Glycerin. If I
were to apply them stronger, I would increase the frit ratio. However, the
stains are very strong without being thick. My colors are very bright and
strong using this method. Your method seems to lean to more stain to your
other material.
Regards,
Bonnie Staffel
http://webpages.charter.net/bstaffel/
http://vasefinder.com/bstaffelgallery1.html
Charter Member Potters Council
| |
|