copper fuming

updated fri 9 sep 05

 

Michele D'Amico on thu 8 sep 05


Is it posible to get copper fuming when firing in oxidation in an electric
kiln?

Des & Jan Howard on fri 9 sep 05


Michele
I don't know how it happens, but, when we are doing slow cools/firedowns,
(glazed pots previously gas fired to Cones 10,11 &/or 12 & refired to
1020C in an electric kiln),
we get copper flashing on some pots closest to the elements, especially
celadon glazed ones.
Des