search  current discussion  categories  techniques - photography 

new ceramic camera photographs

updated sat 10 sep 05

 

Steve Irvine on fri 9 sep 05


In the time since the article in PMI about making a ceramic camera came out I've posted a couple
of new ceramic camera images on my photography site. The ceramic camera used for both of
these photos is basically like a large, lidded caserole that has been cut in half, with a slab added to
the front. It's the cobalt blue one, about half way down this page:
http://www.steveirvine.com/pinhole/cameras.html

One of the new images is a 90 second exposure exterior photo:
http://www.steveirvine.com/pinhole/image170.html

The other is a 90 minute exposure interior photo:
http://www.steveirvine.com/pinhole/image165.html

Steve
http://www.steveirvine.com