Edouard Bastarache Inc. on fri 23 sep 05
Sorry all,
I made a mistake when I wrote the recipe of my C/04 Orange/Red Shino on =
FlickR,
I forgot to write the amount of Silica, I just made the correction and :
Silica.......................7
http://www.flickr.com/photos/potier/20552751/
Later,
"Ils sont fous ces quebecois"
"They are insane these quebekers"
"Est=E1n locos estos quebequeses"
Edouard Bastarache
Irreductible Quebecois
Indomitable Quebeker
Sorel-Tracy
Quebec
edouardb@sorel-tracy.qc.ca
www.sorel-tracy.qc.ca/~edouardb/Welcome.html
http://www.flickr.com/photos/potier/
http://perso.wanadoo.fr/smart2000/index.htm
http://www.digitalfire.com/education/toxicity/
http://www.flickr.com/photos/potier/20552751/
Maurice Weitman on fri 23 sep 05
At 3:18 PM -0400 on 9/23/05, Edouard Bastarache Inc. wrote:
>Sorry all,
>
>I made a mistake when I wrote the recipe of my C/04 Orange/Red Shino
>on FlickR,
>I forgot to write the amount of Silica, I just made the correction and :
>Silica.......................7
Salut, Edouard,
I noticed that it added up to 91, but I thought it was either because
you included the oxides in the total or it had something to do with
the Canadian/US exchange rate.
Or maybe it was another blond shino joke.
What ever.
Regards,
Maurice
| |
|