Paxton on tue 4 oct 05
I'm using this glaze with additions of 5% TiO2 and 5% CuCO3.
the listings I have seen are for oxidation. Has anyone fired this glaze =
in reduction?
If so what differences were there from the oxidation firing?
Thanks
Bill Paxton
Gordon Ward on tue 4 oct 05
I've used the variation called "weathered bronze green" in reduction at
^9/10. There is more mottling/variation and will break some over
texture. I think it's the same as the one you are asking about.
Gordon
On Oct 4, 2005, at 12:42 PM, Paxton wrote:
> I'm using this glaze with additions of 5% TiO2 and 5% CuCO3.
>
> the listings I have seen are for oxidation. Has anyone fired this
> glaze in reduction?
>
> If so what differences were there from the oxidation firing?
>
> Thanks
> Bill Paxton
| |
|