Paul Herman on sat 22 oct 05
Hi Bruce,
Try ALS Chemex. They are worldwide, and have a web page.
http://www.alschemex.com/
I had them do XRF tests on my local materials and was very satisfied.
It was $120.00 for four different specimens. They have several
offices in North America.
Best,
Paul Herman
Great Basin Pottery
Doyle, California US
greatbasinpottery.com
On Oct 19, 2005, at 2:33 PM, Bruce Girrell wrote:
Can anyone recommend a university or testing service where I could get a
mineralogical analysis performed?
How much does such a test cost?
Bruce "good glaze, no recipe" Girrell
| |
|