Pat Southwood on mon 7 nov 05
Hi,
I have done a few of these in the last few months, havibg finally =
convinced my husband that I cant hold up a Clay Bulley and fix it onto =
the wall at the same time!
We always used wood at college, but when I tried it at home mine kept =
splitting along the grain.
I smiled nicely at the 3d technician who gave me some marine ply and =
mdf. They both worked well. I suspect the edges might blur after a while =
with the mdf. It was also suggested that I use 1/8th " perspex.
Hope this helps.
Pat Southwood