PAM EASLEY on thu 10 nov 05
Try putting some newspaper under and lightly over your work, then the =
plastic film. I have kept things nice an moist and workable for up to a =
couple of weeks using this method. Most but not wet. I think this may =
help with the whistle project.
Let us know how you do......... I love whistles and have a heck of a =
time getting them to actually sound good. I applaud you.
Pam in Seattle
Janna Marcilla on fri 11 nov 05
On Thu, 10 Nov 2005 22:04:48 -0800, PAM EASLEY wrote:
>Try putting some newspaper under and lightly over your work, then the
plastic film. I have kept things nice an moist and workable for up to a
couple of weeks using this method. Most but not wet. I think this may help
with the whistle project.
Thanks so much Pam, I will try that this weekend!
Janna
| |
|