search  current discussion  categories  materials - clay 

porcelain. new insights on whiteness & translucency

updated wed 7 dec 05

 

Steve Mills on tue 6 dec 05


I had a quick check and found that the previous Nepheline Syenite was
Norfloat. They removed themselves from the UK craft materials market by
raising the minimum order quantity beyond a feasible limit. Northcape is
now the only one available to us. It is approximately 3 percent lower in
Silica than the other.

Best regards

Steve


In message <002001c5fa2d$770955e0$33d8ebdc@oemcomputer>, Ivor and Olive
Lewis writes
>Dear Steve,
>I did a "Google" on North Cape.
>Reading their Sales Promotional stuff seems to suggest that they are
>doing a lot of separating, beneficiation and blending to get
>consistent products. This can have a colossal effect on production
>costs. In addition, currency exchange rates make things bad for
>importers.
>I would have thought that you might have had some good local deposits
>in the north, Scotland perhaps.
>never the less, the information I put forward should be of interest to
>people who are considering making their own Porcelain bodies.
>Best regards,
>Ivor Lewis.
>Redhill,
>South Australia.
>

--
Steve Mills
Bath