search  current discussion  categories  glazes - specific colors 

opal green from donna

updated sat 10 dec 05

 

Randy McCall on thu 8 dec 05


Donna,,,,,,,,how do you apply the two glazes to get opal green. Bronze
green under Raspberry? How thick?

Randy

Pottery Web Site
members.tripod.com/~McCallJ/index.html
South Carolina


----- Original Message -----
From: "Donna Kat"
To:
Sent: Thursday, December 08, 2005 12:38 AM
Subject: Re: cone 6 glazes with depth


> One of the most used cone 6 glazes that has wonderful depth and interest
> when it is right is Floating Blue. Another is Randy's Red which can be
> quite warm and lovely. Both of these use Gerstley and require a slow
> cooling at around 1000 F for the crystals to develop. Mastering Cone 6
> was
> mentioned and one of the blues given in it looks like floating blue at its
> brightest and doesn't use Gerstley. Another glaze that I like despite
> it's
> settling and turning rock hard when left to sit in the bucket is
> wheathered
> bronze green (pinnell's green?). This with MC6's raspberry can make a
> knock your socks off opal green. Honey is lovely for adding nice touches
> if splattered in the inside of a bowl on top of other glazes (it runs).
> On
> Randys Red it makes gold.
>
> Look under "stability" at -
>
> http://www.frogpondpottery.com/index.shtml
>
> (also has info on MC6)
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>

Donna Kat on fri 9 dec 05


On Thu, 8 Dec 2005 05:45:38 -0500, Randy McCall wrote:

>Donna,,,,,,,,how do you apply the two glazes to get opal green. Bronze
>green under Raspberry? How thick?
>
>Randy
>
>Pottery Web Site
>members.tripod.com/~McCallJ/index.html
>South Carolina

I am really a haphazard glazer. It has been awhile since I used that
combination because I avoid making the raspberry (I don't care for it other
than for this). I am 99% certain it is weathered bronze green over
raspberry. I dip my glazes for the most part and the application of
Pinnell's is on the thick side with the raspberry thin. Honey over
weathered green also gives this look and you don't risk getting the
red/green I dislike if the application misses. You just have to be careful
about running.

http://www.masteringglazes.com/Pages/Updateframe.html

actually has this pictured.