Brad Carter on sun 11 dec 05
Alisa Clausen posted a glaze with 31.7 % iron. Could this be a mistake?
Rosie's Red
cone 6
posted 2-17-05
29.7 silica
5.0 kaolin
19.8 kona feldspar
13.9 talc
31.7 red iron oxide
Brad Carter
Grass Valley, Calif
marianne kuiper milks on sun 11 dec 05
Brad,
The Rosie's Red I have, which is good, is completely different.
Flint 150
Kaolin-EPK 25
Soda F-4 spar 100
Talc 70
Gerstley borate 160
Red iron 75.75
Works both on ^6 and ^7
If you put Albany slip over Rosie's it makes a great grey, green on the edges.
If interested, I have a lovely Rosie's Blue as well.
Good luck, hope I didn't add to frustration. It's a soft blue that works very well oiver/under other glazes, slight satin.
Marianne
Brad Carter wrote: Alisa Clausen posted a glaze with 31.7 % iron. Could this be a mistake?
Rosie's Red
cone 6
posted 2-17-05
29.7 silica
5.0 kaolin
19.8 kona feldspar
13.9 talc
31.7 red iron oxide
Brad Carter
Grass Valley, Calif
______________________________________________________________________________
Send postings to clayart@lsv.ceramics.org
You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/
Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
---------------------------------
Yahoo! Shopping
Find Great Deals on Holiday Gifts at Yahoo! Shopping
| |
|