Gary Harvey on fri 6 jan 06
Floating blue is a difficult glaze to make. It is blue with tiny white
flecks if fired right or horrible green if not. It is brown if too thin and
blue streaked if both thin and thick. (Which is ok I like it this way too.)
It is not a cone 6 glaze it is a cone 5 glaze. AND it must be cooled fast
not slow or it is the horrible green. This is how to make it. click here.
http://www.potters.org/subject16252.htm G. Harvey Palestine TX
----- Original Message -----
From: "Mary/Adams"
To:
Sent: Wednesday, January 04, 2006 5:45 PM
Subject: Floating Blue is like???
> What??????? To a Potter??????
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>
| |
|