Janine LaMaie on tue 10 jan 06


Elizabeth:

To save you the trouble, I tracked this down. From Tony Hansen,
DigitalFire.

G1214Z
WOLLASTONITE 27.00 CaO 0.88*
FRIT 3124 36.00 K2O 0.01*
EPK KAOLIN 35.00 Na2O 0.10*
SILICA 5.00 Al2O3 0.47
======== B2O3 0.19
103.00 SiO2 2.51
Si:Al 5.78 Expan 7.10


Cheers!