search  current discussion  categories  places - far east 

china clay q38

updated sat 21 jan 06

 

Sam Kelly on fri 20 jan 06


Hi, my supplier has increased the cost of raw materials(due to frieght)
and I was wondering, with a bag cost difference of (AUD)$10, is there a
major difference between China Clay Q38 and Kaolin(ekalite 2) when used in
glazes or slip casting bodies- cone9-10 gas reduction. Thanks.

Sam