search  current discussion  categories  glazes - faults 

once a pinhole always a pinhole?

updated sun 22 jan 06

 

Stacey and Gary Ballard on thu 19 jan 06


Hi Everyone,
I have a piece I really like, but after the glaze firing (06) I =
discovered pinholes. Is there any way to reglaze, refire, re-anything =
to fix it? This is my first experience with it, I would like to try and =
save the piece if possible. Any advice? =20

Thank you as always, clayart is a constant gift to my art. From =
technical discussion to heartfelt stories, Clayart is a blessing! Thank =
you all.

Stacey
http://www.basicelements.biz

Gary Harvey on sat 21 jan 06


You could try rubbing glaze into the pin holes and refiring. I have done
this a time or two with success. Gary Harvey, Palestine TX
----- Original Message -----
From: "Stacey and Gary Ballard"
To:
Sent: Friday, January 20, 2006 12:13 AM
Subject: Once a pinhole always a pinhole?


Hi Everyone,
I have a piece I really like, but after the glaze firing (06) I discovered
pinholes. Is there any way to reglaze, refire, re-anything to fix it? This
is my first experience with it, I would like to try and save the piece if
possible. Any advice?

Thank you as always, clayart is a constant gift to my art. From technical
discussion to heartfelt stories, Clayart is a blessing! Thank you all.

Stacey
http://www.basicelements.biz

______________________________________________________________________________
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.