Gina Mars on sun 29 jan 06
I am looking for advise on where and what kind of kiln shelves I should
purchase for my Alpine 16 cubic kiln. The shelves are 11 by 28 and are
quite expensive. I have heard about the ultra lite shelves. I will fire to
cone 10. Any info would be greatly appreciated. Thanks, Gina
www.marspottery.net
William & Susan Schran User on tue 31 jan 06
On 1/29/06 8:09 PM, "Gina Mars" wrote:
> I am looking for advise on where and what kind of kiln shelves I should
> purchase for my Alpine 16 cubic kiln. The shelves are 11 by 28 and are
> quite expensive. I have heard about the ultra lite shelves.
Oh man, you think shelves are expensive, wait until you find out the price
of those "ultra lite" shelves!
Here's a link for one source:
http://www.kilnshelf.com/pages/387847/index.htm
I've received 20 Advancer shelves from them. Two shipments, two boxes each
shipment, very well packed & insured, shipped UPS, nothing broken.
Very happy to replace my old heavy silicon carbide shelves.
-- William "Bill" Schran
Fredericksburg, Virginia