geil nitrdde bond shelves?

updated sat 11 feb 06

 

john tracey on thu 9 feb 06


Has any one out there been using Geils nitride bonded shelves? If so
any reviews would be appreciated.
Thanks, John Tracey

Mark Issenberg on fri 10 feb 06


Ive been using them ,, I spread alumina not kiln wash and i really like the
kilns , so much lighter than my other shelves

Mark
Lookout Mountain Pottery

john tracey on fri 10 feb 06


Mark ,thanks for the reply. how long have you used them,and what temp
do you fire to. Have they remained flat? no warping? Or cracking?
On Feb 10, 2006, at 9:05 AM, Mark Issenberg wrote:

> Ive been using them ,, I spread alumina not kiln wash and i really
> like the
> kilns , so much lighter than my other shelves
>
> Mark
> Lookout Mountain Pottery
>
> _______________________________________________________________________
> _______
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>

Mark Issenberg on fri 10 feb 06


Hi ya,, i fire cone 10.. they are flat and just like when they were new,,
Ive fired them 5 or 6 times or more

Mark