Allyson May on fri 17 feb 06


Thanks to everyone who responded to my frit question. I had decided =
that 3195 was the best place to start looking at the little info I did =
have on my available frits. I am fiddling with a Bailey glaze from the =
Cone 6 Glaze Book which calls for a low expansion frit but does not say =
which one. I sat down with all the frits I had and crossed out the =
obvious no's and was left with the 3 I asked about. Its good to know =
that my intuition was leading me down the right path. I will be running =
some tests this week. Thanks again!!
Peace,
Allyson May
Stoney Creek Pottery
Bloomington, IN