heidi h on tue 21 feb 06
dawn.
in my experience...2 or 3 percent cobalt is way overkill. i use .85
%cobalt carb and 2.5% copper carb for a lovely deep blue. the base
dependes if you want matte
or glossy. i have one of each in my palette.
good luck.
heidi haugen west glacier.montana.usa
| |
|