search  current discussion  categories  tools & equipment - misc 

axner=?iso-8859-1?b?uq==?=s clay substitutes for miami clays

updated fri 24 feb 06

 

Rosanne on thu 23 feb 06


Hello All,

I wanted to forward the Axner's Clay Substitution for Miami Clay:

#1 TURNER PORCELAIN:
Norma=B9s Porcelain for (cone 9-10)
Mary=B9s Porcelain for (cone 5-6)

#1A English Porcelain:
Norma=B9s Porcelain (cone 5-6)

#2 Steve=B9s Stoneware:
Karen=B9s Stoneware (cone 9-10)
Josh=B9s Stoneware (cone 9-10)
Tom Sawyer=B9s Sand Stoneware (cone 9-10)
Jepson Stoneware (cone 9-10)
Sophie=B9s Stoneware (darker) (cone 9-10)

#3 Ken=B9s Sculpt Clay:
Max=B9s Sculpture Clay (white) (cone 06-10)
Bob=B9s Tile & Sculpture (toasty) (cone 06-10)

#5 Almond Stoneware:
Karen=B9s Stoneware (cone 9-10)
Josh=B9s Stoneware (cone 9-10)
Tom Sawyer=B9s Sand Stoneware (cone 9-10)
Jepson Stoneware (cone 9-10)

#6 Elmer=B9s Peachy Buff:
Sybil=B9s Stoneware VI (whiter than peach) (cone 5-6)
Autumn=B9s Stoneware VI (whiter than peach) (cone 5-6)
Rae=B9s Smooth Stoneware (whiter than peach) (cone 5-6)

#7 White Earthenware:
Sybil=B9s Stoneware VI (cone 5-6)
Autumn=B9s Stoneware VI (cone 5-6)
Rae=B9s Smooth Stoneware (cone 5-6)

#8 Toasty Orange Clay:
Elisabeth=B9s Stoneware VI (cone 5-6)
Mike=B9s Stoneware VI (cone 5-6)

#9 Red Earthenware:
Stanley=B9s Red (cone 06-02)
Sid=B9s Red Majolica (cone 06-02)
Rojo Linda (cone 06-02)
Carolyn=B9s PHB (cone 06-02)
Steve & Linda=B9s Red (cone 06-02)

#10 Mark=B9s Speckled Brown:
Elisabelth=B9s Stoneware VI with Speckles (cone 5-6)

#11 White Talc Body:
Vince=B9s Low White (cone 06-02)
Wade=B9s Low White (cone 06-02)

#11M White Talc w/Sand:
Vince=B9s Low White with Grog (cone 06-02)
Wade=B9s Low White with Grog (cone 06-02)

#12 Jan=B9s Dark Brown:
Nothing exactly similar but try Elisabeth=B9s Stoneware VI (cone 5-6)

#14 Raku:
Max=B9s Raku (cone 06-10)
Sylvia=B9s Raku (cone 06-6)
Elena=B9s Raku cone (cone 06-2)

#15 Black Clay:
Nothing exactly similar but try Axner Black Colored Porcelain for small
forms (cone 5-6)

#16 Ellies White Stoneware:
Mark=B9s White Stoneware (cone 9-10)
Brooke=B9s White Stoneware (cone 9-10)

#17 Lizella Clay:
Rojo Linda for lower temperatures (06 =AD 02)
Sophie=B9s Orange (cone 10)
Bob=B9s Tile & Sculpture (cone 6)

#18 Econo Clay:
Axner Purge in different temperature versions

I hope this helps.

If anyone would like a FREE sample of any of our clay bodies, give us a cal=
l
1-800-843-7057.

Create, sculpt, fire-up!
Rosanne Sloane
Education Coordinator
Axner.com=20
1-800-843-7057 x231
rosanne@axner.com
490 Kane Court Oviedo, FL 32765



on 2/23/06 1:34 PM, Lynne Antone at bvrcrkarts@COMCAST.NET wrote:

> Hi all,
>=20
> When I told a friend about Miami Clay Co. going out of business, she aske=
d if
> I would query the group with this:
>=20
> <> if anyone knows whether or not the #11 talc clay will be produced by
> someone else now that he is out of business. Or if anyone else has the
> recipe??? I could get someone else to make it if I could get the recipe.=
>>
>=20
> Thanks for any help with this,
> Lynne Antone
> --
> Beaver Creek Arts
> Olympia WA
> USA
>=20
> _________________________________________________________________________=
_____
> Send postings to clayart@lsv.ceramics.org
>=20
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>=20
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>=20