June Perry on sun 26 feb 06
Bonnie,
I'd be prone to try adding a bit of high bearing fireclay like Newman red.
It will add some more iron and that might help retain the color you want.
You can adjust it for more or less color by adding more or lessening it and
adding some lower iron bearing clay.
Warm regards,
June Perry
_http://www.angelfire.com/art2/shambhalapottery/_