c 6 celadon

updated tue 28 feb 06

 

Lili Krakowski on mon 27 feb 06


Saying this up front: I do not do reduction firing, have not tested this.

From Emmanuel Cooper's wonderful "The Potter's Book of Glaze Recipes"

#138
Neph Sy. 36
Calcium borate frit
(colemanite) 7
Dolomite 10
Zinc Oxide 3
Barium Carbonate 7
Bentonite 3
Flint 34
Tin Oxide 1%
Red Iron Oxide 1%

"A clear transparent glaze in oxidation, smooth and even over a wide
temperature range. In reduction it gives a pale green on stoneward, a
delicate 'baby blue' on porcelain."

NOTE THAT THIS GLAZE USES BARIUM WHICH I WOULD REPLACE BY STRONTIUM OR
CALCIUM.

From Michael Bailey's gorgeous "Oriental Glazes" (featuring inter al some
breathtaking Marcia Selsors) there is the definition that a celadon is a
transparent or semi-transparent glaze in reduction--to which a bit of iron
has been added, or which picks up a bit of iron from the body. He adds that
iron introduced into the glaze is added as red iron oxide, or as a little
red clay...

So I would go with that...and test.