search  current discussion  categories  materials - misc 

egyptian paste 3

updated thu 9 mar 06

 

Centa Uhalde on wed 8 mar 06


Thanks, Lili, for the feedback. I will look in my library for more info. I
have had this recipe in the perennial paper pile on my desk that I pulled
from somewhere off the internet. Don't know what temp to fire at, but I will
post it here in case there is comment, or someone else wants to explore.
What's the difference between it and an engobe or slip? I imagine it is not
just a surface cover, more integrated with clay body emerging from the
interaction?

Vivika's Egyptian Paste

Kona F-4 Spar 684
Soda Ash 130
Soda Bicarb 130
Kaolin 210
Flint 684
Bentonite 30

This quantity will fit in a gallon jug.

Thanks,