Lili Krakowski on fri 17 mar 06


Sorry: I wrote " The most plastic [slips] (biggest clay content) go on
earthernware, and the least plastic (more flint) on bisque. "

What I should have written is that the most plastic go on LEATHERHARD (or
softer) clay etc. (Of course there are temperature adjustments too, subject
of the earlier discussion of slips this week.)

Apologies

Lili Krakowski