search  current discussion  categories  glazes - cone 4-7 

cone 6 version karen's starshine

updated mon 8 may 06

 

Alisa Liskin Clausen on sun 7 may 06


This glaze looks particularly nice on dark claybodies.

The ^6 recipe is in the archives as well as many others, just in case in
the future someone is looking for cone 6 glaze recipes to experiment with.

Best regards from Alisa in Denmark