search  current discussion  categories  glazes - misc 

page 6 glaze tests

updated wed 10 may 06

 

Randy McCall on sun 7 may 06


For those interested I have added Page 6 of my glaze tests to my web site.

Just click the site below and go to the Potter's Corner. To get back to the
main page after viewing a test page, just close the test page.

Randy
South Carolina
Pottery Web site

http://members.tripod.com/~McCallJ/index.html

John Post on sun 7 may 06


Hi Randy,

i think your glaze test page might be more useful if you were to include
the recipes for the glazes on the same page that the test results are on.

John Post

Randy wrote:

>For those interested I have added Page 6 of my glaze tests to my web site.
>
>South Carolina
>Pottery Web site
>http://members.tripod.com/~McCallJ/index.html
>
>

Randy McCall on mon 8 may 06


John,,,,,,,,,you are right,,,,,,,, but you will have to either search the
archives in Clay
Art, get the Ceramics Monthly magazine for Sept 2005 that has Jane Shatz
recipes or buy the two Cone 6 books that the glazes came out of to get the
recipes from the books. Some of the recipes for these glazes are not
considered public by the authors.