Hey Fred,

Look in the archives for Wayne's Blue. This is a killer Noxema type =
blue. I use it and don,t have any problems with pinholes, crazing,..... =
I fire ^6 on porcelain using RR and John's firing schedule. If you =
can't find it let me know and I will send the recipe to you.