search  current discussion  categories  safety - health 

allergies to glazes? part ii

updated fri 2 jun 06

 

Mary Adams on thu 1 jun 06


Yes, I have a really good respirator that I got from Galeton.

Malcolm Schosha on thu 1 jun 06


Well, is your skin coming in contact with any un-fritted glaze
ingredients; either dry or wet? That can be a major problem.

Malcolm

...............................



--- In clayart@yahoogroups.com, Mary Adams wrote:
>
> Yes, I have a really good respirator that I got from Galeton.
>
>
______________________________________________________________________
________
> Send postings to clayart@...
>
> You may look at the archives for the list or change your
subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@...
>