search  current discussion  categories  glazes - misc 

unusual glaze ingredient

updated fri 2 jun 06

 

J Lutz on thu 1 jun 06


A spring cleaning resulted in finding some VERY old eye shadow.
I rubbed some on a small textured tile and it survived a ^6 firing.

So now I'm going to try using it in a clear glaze and see what
happens. The resulting colors weren't the same as the eye shadow but
at least there was color remaining which surprised me.

Of course there is not ingredient list on the little case so I have
no idea what it's made of. Probably don't really want to know!

Jean Lutz
Prescott, AZ