Randy McCall on sun 4 jun 06
I have done some tests on glaze test tubes and there was a definite large
reduction in the number of pinholes when I washed the tubes before dipping.
That was on a glaze that was having a lot of pinholes for me. It did make a
difference, but did not totally eliminate the pinholing.
Randy