Tom at Hutchtel.net on fri 23 jun 06
For whatever reason, Ron, my replies to your email is getting blocked. So
unfortunately I'm replying through the list.
Tom
Hi Ron...
Yes definitely include us. Whatever we can add to the storehouse we'll be
glad to.
One reason I mentioned test bar dimensions, is that I'd theorize that bar
size can also vary the results. To Thick and you might not get penetration.
Tom
Ron Roy on sat 24 jun 06
Hi Tom,
You are added.
One reason for doing the research is to find out what it takes for thicker
samples - to saturate completely.
Some samples will be 1/2 inch thick for instance. The larger the sample the
more accurate the results will be - we already know that.
I have not seen your emails in my spam box so I don't know what is
happening to them - have you checked with your server?
RR
>For whatever reason, Ron, my replies to your email is getting blocked. So
>unfortunately I'm replying through the list.
>
>Tom
>
>Hi Ron...
>Yes definitely include us. Whatever we can add to the storehouse we'll be
>glad to.
>
>One reason I mentioned test bar dimensions, is that I'd theorize that bar
>size can also vary the results. To Thick and you might not get penetration.
>
>Tom
Ron Roy
RR#4
15084 Little Lake Road
Brighton, Ontario
Canada
K0K 1H0
| |
|