We mixed up a ^10 celadon today and mistakenly added red copper oxide instead of iron. Dang.
Can any of you glaze experts anticipate what will happen with this? I will go ahead and test it.
Help please.
jude

cornwall stone 60
Grolleg 11
Wollastonite 17
dolomite 6
Flint 325 6
RIO .5



617-547-5513
jmotzkin at yahoo.com
http://www.motzkin.com
http://spiritkeeper-urns.com

---------------------------------
Yahoo! Messenger with Voice. Make PC-to-Phone Calls to the US (and 30+ countries) for 2¢/min or less.

Daniel Semler on fri 7 jul 06


Hi Jude,

My guess, and that's all it is, would be some form of copper red, as I'm
assuming you're firing this in reduction given that its a celadon. I would not
expect a great red though given the high alumina content.

Let us know the results of your test.

Thanx
D