Doug Carpenter on fri 7 jul 06


I am in need of a ^6, matt or semi-matt cucumber green glaze recipe. I =
can not find one in the archives or on the web.
Thanks.

William & Susan Schran User on sat 8 jul 06


On 7/7/06 5:27 PM, "Doug Carpenter" wrote:

> I am in need of a ^6, matt or semi-matt cucumber green glaze recipe.

I'm eating cucumbers from my garden and I studied a few attempting to decide
which green you are searching for as the cucumbers are variegated green. I
also grow white cucumbers!

I you want a very specific color, start with a reliable transparent glaze
and add a stain in the color that closely matches your search.

Here's a link to the Mason Color green stains:
http://www.masoncolor.com/newfiles/greens.html


-- William "Bill" Schran
Fredericksburg, Virginia
wschran@cox.net
wschran@nvcc.edu

June Perry on sat 8 jul 06


You didn't mention what part of the cucumber -- skin or fruit???

I have a lovely C6 dark green gloss on my web page at:

_www.angelfire.com/art2/shambhalapottery_
(http://www.angelfire.com/art2/shambhalapottery)

Just scroll down the page and hit the links for the cone 6 recipe and test
tile photo pages.

There's also a lovely high calcium matt light green if that's the color
you're looking for.

Regards,
June Perry
_www.angelfire.com/art2/shambhalapottery_
(http://www.angelfire.com/art2/shambhalapottery)

blog:
_http://shambhalapottery.blogspot.com_ (http://shambhalapottery.blogspot.com)