fw: burn off wax resist?

updated tue 11 jul 06

 

Bonnie Hellman on mon 10 jul 06


Randy,

When I get wax resist where I don't want it, I usually put it in my kitchen
oven at around 300 or maybe 350 (although I think it burns off cooler than
that). Then I come back to it after a while, let the pot cool enough to
glaze, and go on with the rest of the pots.

The short answer is: Not Very. If you put it in your kitchen oven, you'll
smell the wax quite soon.

Bonnie


>
> ----- Original Message -----
> From: "Randy McCall"
> To:
> Sent: Monday, July 10, 2006 6:42 AM
> Subject: Burn Off Wax Resist?
>
>
>> How high do you have to get a kiln to burn off wax resist?
>>
>>
>> Randy
>> South Carolina
>> Pottery Web site
>>
>> http://members.tripod.com/~McCallJ/index.html
>>
>> ______________________________________________________________________________
>> Send postings to clayart@lsv.ceramics.org
>>
>> You may look at the archives for the list or change your subscription
>> settings from http://www.ceramics.org/clayart/
>>
>> Moderator of the list is Mel Jacobson who may be reached at
>> melpots@pclink.com.
>